- W1003341306 startingPage "199" @default.
- W1003341306 abstract "用自制的销环式腐蚀磨损试验机测定了 Fe-Ni-Cr(Mo,Cu)合金在20%H_2SO_4溶液中腐蚀、阴保、钝化及过钝化等电位区的腐蚀磨损-载荷关系,用 SEM 观察了磨痕。结果表明,材料流失量远大于18-8不锈钢,而且主要是磨损造成的。合金中 Ni 的含量高,降低了形变强化能力,是耐磨性下降的原因。" @default.
- W1003341306 created "2016-06-24" @default.
- W1003341306 creator A5017065041 @default.
- W1003341306 creator A5049939880 @default.
- W1003341306 creator A5066727596 @default.
- W1003341306 creator A5088502213 @default.
- W1003341306 date "1992-06-25" @default.
- W1003341306 modified "2023-09-24" @default.
- W1003341306 title "Fe-Ni-Cr(Mo,Cu)合金的腐蚀磨损行为" @default.
- W1003341306 hasPublicationYear "1992" @default.
- W1003341306 type Work @default.
- W1003341306 sameAs 1003341306 @default.
- W1003341306 citedByCount "0" @default.
- W1003341306 crossrefType "journal-article" @default.
- W1003341306 hasAuthorship W1003341306A5017065041 @default.
- W1003341306 hasAuthorship W1003341306A5049939880 @default.
- W1003341306 hasAuthorship W1003341306A5066727596 @default.
- W1003341306 hasAuthorship W1003341306A5088502213 @default.
- W1003341306 hasConcept C191897082 @default.
- W1003341306 hasConcept C192562407 @default.
- W1003341306 hasConceptScore W1003341306C191897082 @default.
- W1003341306 hasConceptScore W1003341306C192562407 @default.
- W1003341306 hasIssue "3" @default.
- W1003341306 hasLocation W10033413061 @default.
- W1003341306 hasOpenAccess W1003341306 @default.
- W1003341306 hasPrimaryLocation W10033413061 @default.
- W1003341306 hasVolume "6" @default.
- W1003341306 isParatext "false" @default.
- W1003341306 isRetracted "false" @default.
- W1003341306 magId "1003341306" @default.
- W1003341306 workType "article" @default.