- W271094312 endingPage "1173" @default.
- W271094312 startingPage "1169" @default.
- W271094312 abstract "Fe-Nb-C合金内耗测试表明:700℃,1 h水淬合金的Snoek峰较低,而且含Nb越多,Snoek峰高(hs)越低.与通常铁基材料不同,变形导致Fe-Nb-C合金的hs增强:对于含Nb(≥0.06%,质量分数,下同)较低的合金,'Snoek阻尼温区'(室温-150℃)内耗增强显著,其Snoek峰高温支明显抬起、甚至形成混合双峰;对于含Nb≥0.3%的合金,hs增强甚微,仍是一对称的Snoek峰,并在80-130℃间形成-分立峰.降温SKK峰向低温移动,但峰高(hcsKK)未减低,含Nb较低合金的hcSKK都明显高于hhSKK." @default.
- W271094312 created "2016-06-24" @default.
- W271094312 creator A5040882983 @default.
- W271094312 creator A5059381927 @default.
- W271094312 date "2001-11-18" @default.
- W271094312 modified "2023-09-28" @default.
- W271094312 title "Fe-Nb-C合金的中温内耗" @default.
- W271094312 hasPublicationYear "2001" @default.
- W271094312 type Work @default.
- W271094312 sameAs 271094312 @default.
- W271094312 citedByCount "0" @default.
- W271094312 crossrefType "journal-article" @default.
- W271094312 hasAuthorship W271094312A5040882983 @default.
- W271094312 hasAuthorship W271094312A5059381927 @default.
- W271094312 hasConcept C41008148 @default.
- W271094312 hasConceptScore W271094312C41008148 @default.
- W271094312 hasIssue "11" @default.
- W271094312 hasLocation W2710943121 @default.
- W271094312 hasOpenAccess W271094312 @default.
- W271094312 hasPrimaryLocation W2710943121 @default.
- W271094312 hasVolume "37" @default.
- W271094312 isParatext "false" @default.
- W271094312 isRetracted "false" @default.
- W271094312 magId "271094312" @default.
- W271094312 workType "article" @default.