- W804143192 abstract "采用表面腐蚀、慢应变速率拉伸(SSRT)实验研究预拉伸变形对Al-Cu-Mg合金腐蚀性能的影响。利用扫描电镜观察分析Al-Cu-Mg合金断口形貌及结构。结果表明,预拉伸变形可显著提高合金位错密度,为H原子的扩散提供更多的通道,因此,在相同腐蚀时间下,3.5%Na Cl溶液中T8态Al-Cu-Mg合金的腐蚀速率高于T6态。此外,预拉伸变形可显著增加S相弥散度,使得S相两侧的无沉淀析出带变窄,有效降低了晶界和晶内的电位差,从而降低晶界沉淀相的溶解速度,因此,在同一热处理状态下,Al-Cu-Mg合金在饱和H2S溶液中的应力腐蚀开裂敏感性高于干燥空气中的腐蚀开裂敏感性。同一应变速率下,T8态Al-Cu-Mg合金具有比T6态更好的抗应力腐蚀性能,表明预拉伸变形处理可显著提高合金的抗应力腐蚀性能。" @default.
- W804143192 created "2016-06-24" @default.
- W804143192 creator A5002420233 @default.
- W804143192 creator A5008472138 @default.
- W804143192 creator A5011427831 @default.
- W804143192 creator A5013899804 @default.
- W804143192 creator A5079774126 @default.
- W804143192 date "2015-01-01" @default.
- W804143192 modified "2023-09-24" @default.
- W804143192 title "预拉伸变形对Al-Cu-Mg合金腐蚀性能的影响" @default.
- W804143192 hasPublicationYear "2015" @default.
- W804143192 type Work @default.
- W804143192 sameAs 804143192 @default.
- W804143192 citedByCount "0" @default.
- W804143192 crossrefType "journal-article" @default.
- W804143192 hasAuthorship W804143192A5002420233 @default.
- W804143192 hasAuthorship W804143192A5008472138 @default.
- W804143192 hasAuthorship W804143192A5011427831 @default.
- W804143192 hasAuthorship W804143192A5013899804 @default.
- W804143192 hasAuthorship W804143192A5079774126 @default.
- W804143192 hasConcept C41008148 @default.
- W804143192 hasConceptScore W804143192C41008148 @default.
- W804143192 hasIssue "1" @default.
- W804143192 hasLocation W8041431921 @default.
- W804143192 hasOpenAccess W804143192 @default.
- W804143192 hasPrimaryLocation W8041431921 @default.
- W804143192 hasVolume "20" @default.
- W804143192 isParatext "false" @default.
- W804143192 isRetracted "false" @default.
- W804143192 magId "804143192" @default.
- W804143192 workType "article" @default.