- W868712280 endingPage "42" @default.
- W868712280 startingPage "40" @default.
- W868712280 abstract "研究了含氮,铌和稀土的Fe-Cr-Ni耐热钢的力学性能和高温特性。结果表明,0.14%N,0.08%RE,0.15%Nb,23%-30%Cr和11%-16%Ni材料经1100℃水淬,1000℃时效热处理,在本试验条件下;具有最佳的综合性能;该材料1000℃时抗氧化性与40Cr25Ni20相当,优于35Cr18Ni25Si2等常用耐热钢。" @default.
- W868712280 created "2016-06-24" @default.
- W868712280 creator A5006062657 @default.
- W868712280 creator A5087229053 @default.
- W868712280 date "1999-01-01" @default.
- W868712280 modified "2023-09-24" @default.
- W868712280 title "锅炉燃烧器喷咀用含N,Nb,RE耐热钢的研究" @default.
- W868712280 hasPublicationYear "1999" @default.
- W868712280 type Work @default.
- W868712280 sameAs 868712280 @default.
- W868712280 citedByCount "0" @default.
- W868712280 crossrefType "journal-article" @default.
- W868712280 hasAuthorship W868712280A5006062657 @default.
- W868712280 hasAuthorship W868712280A5087229053 @default.
- W868712280 hasConcept C41008148 @default.
- W868712280 hasConceptScore W868712280C41008148 @default.
- W868712280 hasIssue "4" @default.
- W868712280 hasLocation W8687122801 @default.
- W868712280 hasOpenAccess W868712280 @default.
- W868712280 hasPrimaryLocation W8687122801 @default.
- W868712280 hasVolume "23" @default.
- W868712280 isParatext "false" @default.
- W868712280 isRetracted "false" @default.
- W868712280 magId "868712280" @default.
- W868712280 workType "article" @default.