- W910877977 endingPage "1816" @default.
- W910877977 startingPage "1814" @default.
- W910877977 abstract "以异佛尔酮二异氰酸酯(IPDI)、聚四氢呋喃二醇(PTMG)、γ-(甲基丙烯酰氧基)丙基三甲氧基硅烷(MEMO)为基本原料,制备了硅烷改性聚氨酯乳液,并外加氮丙啶进一步提高了胶膜的性能。衰减全反射傅里叶变换红外光谱(ATR-FT-IR)对产物的结构进行了表征,考察了MEMO含量对乳液粒径、胶膜耐水性、力学性能及热性能的影响,同时对胶膜的结晶性及接触角进行了测试。结果表明ATR-FT-IR证实了MEMO成功地反应到了聚氨酯分子链上;在m(MEMO)=5.67%,m(AZ)=2%时,胶膜的耐水性最低为14.84%,胶膜的最大拉伸强度为17.334MPa,断裂伸长率为232.56%,改性后聚氨酯的热稳定性提高,结晶性及表面能均降低。" @default.
- W910877977 created "2016-06-24" @default.
- W910877977 creator A5002664168 @default.
- W910877977 creator A5058349180 @default.
- W910877977 creator A5064983809 @default.
- W910877977 date "2011-01-01" @default.
- W910877977 modified "2023-09-24" @default.
- W910877977 title "γ-(甲基丙烯酰氧基)丙基三甲氧基硅烷改性聚氨酯的研究" @default.
- W910877977 hasPublicationYear "2011" @default.
- W910877977 type Work @default.
- W910877977 sameAs 910877977 @default.
- W910877977 citedByCount "0" @default.
- W910877977 crossrefType "journal-article" @default.
- W910877977 hasAuthorship W910877977A5002664168 @default.
- W910877977 hasAuthorship W910877977A5058349180 @default.
- W910877977 hasAuthorship W910877977A5064983809 @default.
- W910877977 hasConcept C41008148 @default.
- W910877977 hasConceptScore W910877977C41008148 @default.
- W910877977 hasIssue "10" @default.
- W910877977 hasLocation W9108779771 @default.
- W910877977 hasOpenAccess W910877977 @default.
- W910877977 hasPrimaryLocation W9108779771 @default.
- W910877977 hasVolume "42" @default.
- W910877977 isParatext "false" @default.
- W910877977 isRetracted "false" @default.
- W910877977 magId "910877977" @default.
- W910877977 workType "article" @default.