- W930642008 abstract "采用新型的喷射沉积工艺制备了Al-3.8Li-0.8Mg-0.4Cu-0.13Zr合金,对合金的拉伸发育豚断裂行为进行了研究。实验结果表明,喷射沉积Al-Li合金经190℃,10h时效后达到峰时效状态,此时材料的综合性能最优,固溶淬火态实验合金拉伸断口为完全穿晶韧窝型。" @default.
- W930642008 created "2016-06-24" @default.
- W930642008 creator A5039368842 @default.
- W930642008 creator A5053063863 @default.
- W930642008 creator A5056509753 @default.
- W930642008 creator A5059112220 @default.
- W930642008 creator A5069913395 @default.
- W930642008 date "1996-02-18" @default.
- W930642008 modified "2023-09-28" @default.
- W930642008 title "喷射沉积Al-3.8Li-0.8Mg-0.4Cu-0.13Zr合金的拉伸断裂行为" @default.
- W930642008 hasPublicationYear "1996" @default.
- W930642008 type Work @default.
- W930642008 sameAs 930642008 @default.
- W930642008 citedByCount "0" @default.
- W930642008 crossrefType "journal-article" @default.
- W930642008 hasAuthorship W930642008A5039368842 @default.
- W930642008 hasAuthorship W930642008A5053063863 @default.
- W930642008 hasAuthorship W930642008A5056509753 @default.
- W930642008 hasAuthorship W930642008A5059112220 @default.
- W930642008 hasAuthorship W930642008A5069913395 @default.
- W930642008 hasConcept C71924100 @default.
- W930642008 hasConceptScore W930642008C71924100 @default.
- W930642008 hasIssue "2" @default.
- W930642008 hasLocation W9306420081 @default.
- W930642008 hasOpenAccess W930642008 @default.
- W930642008 hasPrimaryLocation W9306420081 @default.
- W930642008 hasVolume "32" @default.
- W930642008 isParatext "false" @default.
- W930642008 isRetracted "false" @default.
- W930642008 magId "930642008" @default.
- W930642008 workType "article" @default.